Cast nickel superalloys are supplied as vacuum master alloy ingots and investment castings for gas turbine blades, nozzle guide vanes and integral wheels.
What are Cast Superalloys alloys?
Cast nickel superalloys are supplied as vacuum master alloy ingots and investment castings for gas turbine blades, nozzle guide vanes and integral wheels. This index lists 1 technical articles covering composition, mechanical properties, temperature limits, corrosion behaviour and welding practice for each grade.
Cast nickel superalloys are supplied as vacuum master alloy ingots and investment castings for gas turbine blades, nozzle guide vanes and integral wheels. Hangbo Alloy Group stocks and supplies these grades in round bar, seamless tube, plate, sheet, precision strip, forging, wire and machined-part forms, with mill test certificates to EN 10204 3.1 / 3.2.
| Grade | UNS | Type | Summary |
|---|---|---|---|
| Inconel 713C: Investment Casting Superalloy for Gas Turbine Blades & Vanes | UNS N07713 | Grade guide | Complete technical guide to Inconel 713C (UNS N07713). Chemical composition, mechanical properties, casting characteristics, microstructure. |
Round bars · Seamless tubes · Plates & sheets · Precision strips · Forgings & rings · Welding wire. Not every grade is stocked in every form — cast superalloys, for example, are supplied as master alloy ingots and investment castings rather than wrought bar. Contact us for current stock and size ranges.
Supplied to ASTM, ASME, AMS, DIN/W.Nr., EN, GB and GOST specifications. The individual grade articles list the applicable standard numbers for each product form.
A cast nickel superalloy is supplied as vacuum master alloy ingot and investment-cast into near-net-shape hot-section components; these grades are not wrought into bar, plate or tube.
Inconel 713C (UNS N07713, AMS 5377) is used for integral turbine wheels and nozzle guide vanes where high creep strength and castability are required.
713LC is the low-carbon variant (maximum about 0.05% carbon), giving improved ductility, thermal-fatigue resistance and weldability compared with 713C.
Inconel 738LC (UNS N07738, AMS 5410) is a high-chromium cast grade designed for hot-corrosion-resistant gas turbine blades and vanes.
Most cast superalloys have limited weldability and are usually repaired with specialised procedures; 713LC is notably more weldable than 713C.
Inconel · Hastelloy · Monel · Incoloy · Pure Nickel · Copper-Nickel — see the full family index.